ArticleBMC oral health2022
Effect of erosive media on microhardness and fracture toughness of CAD-CAM dental materials.
Article in BMC oral health, 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 12 papers, 1 of them a synthesis that pooled it.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
12 citing papers in PubMed, 1 synthesis or guideline pooled it, 33 citations in OpenAlex.
- Effect of gastric juice on the surface, optical, and mechanical properties of different computer-aided design/computer-aided manufacturing dental ceramics: A systematic review and meta-analysis.Journal of Indian Prosthodontic Society · 2025Pooled it
- Fracture resistance of premolar screw-retained implant-supported hybrid abutment crowns with monolithic restorations after thermomechanical aging.The journal of advanced prosthodontics · 2026Article
- Influence of crystallization and adhesive cementation on the fracture resistance of CAD/CAM advanced lithium disilicate and zirconia-reinforced lithium silicate ceramics after thermocycling.Frontiers in dental medicine · 2026Article
- Surface roughness and biofilm formation on tooth-colored restorative materials immersed in food-simulating liquids.BMC oral health · 2025Article
- Effect of Simulated Gastric Acid on Surface Characteristics and Color Stability of Hybrid CAD/CAM Materials.Polymers · 2025Article
- The Effect of Erosive Media on Color Stability, Gloss, and Surface Roughness of Monolithic CAD/CAM Materials Subjected to Different Polishing Methods.Scientific reports · 2025Article
- The Effect of Acidic Immersion Media on the Flexural Properties of a High-Performance Fiber-Reinforced CAD/CAM Technopolymer.Polymers · 2025Article
- Gastric acid challenge: Mechanical proficiency and surface gloss of tooth-colored restorative materials.BMC oral health · 2025Article
- Optimizing cleaning procedures for MEP residues: insights from a novel HPLC-MS analysis.Clinical oral investigations · 2025Article
- The Effect of Erosive Media on the Mechanical Properties of CAD/CAM Composite Materials.Journal of functional biomaterials · 2024Article
- Comparative Study of the Influence of Heat Treatment on Fracture Resistance of Different Ceramic Materials Used for CAD/CAM Systems.Materials (Basel, Switzerland) · 2024Article
- The Effect of Home and In-Office Bleaching on Microhardness and Color of Different CAD/CAM Ceramic Materials.Materials (Basel, Switzerland) · 2022Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
3 authors at 1 institution in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
backgroundErosive acids might create surface flaws and deteriorate the mechanical properties of CAD-CAM materials. This invitro study aimed to investigate the effect of simulated gastric HCl and extrinsic erosive acids on surface microhardness and fracture toughness of CAD-CAM materials.
methods400 bar-shaped specimens (17×4×2 mm
resultsErosive media created surface flaws that lowered the surface microhardness of the material and initiated the fracture pattern under different loads according to material type. The material type was a more predominant factor than erosive media that affected either the microhardness or the fracture toughness of CAD-CAM dental materials. The highest VHN and K
conclusionAll CAD-CAM materials used, except Vita Enamic, showed high resistance against the erosive acids indicating higher longevity of the material in patients frequently exposed to either extrinsic or intrinsic acid.