ArticlePolymers2022
Aging Behaviors of Phenol-Formaldehyde Resin Modified by Bio-Oil under Five Aging Conditions.
Article in Polymers, 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
3 citing papers in PubMed, 13 citations in OpenAlex.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
5 authors at 2 institutions in 1 country.
Funding
Abstract
The bio-oil phenol-formaldehyde (BPF) resin, prepared by using bio-oil as a substitute for phenol, has similar bonding strength but lower price to phenol-formaldehyde (PF) resin. As a common adhesive for outdoor wood, the aging performance of BPF resin is particularly important. The variations in mass, bonding strength, microstructure, atomic composition, and chemical structure of BPF resin under five aging conditions (heat treatment, water immersion, UV exposure, hydrothermal treatment, and weatherometer treatment) were characterized by scanning electron microscope, X-ray photoelectron spectroscopy, and Fourier transform infrared spectroscopy, respectively. Compared under five aging conditions, after aging 960 h, the mass loss of plywood and film was largest under hydrothermal treatment; the bonding strength of plywood, the surface roughness, and O/C ratio of the resin film changed most obviously under weatherometer treatment. FT-IR analysis showed that the decreased degree of peak intensity on CH
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.