Zeolite Socony Mobil-Five Coating on Ti-24 Nb-4 Zr-7.9 Sn Promotes Biocompatibility and Osteogenesis In Vitro and In Vivo.
Article in BioMed research international, 2021. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed, 2 citations in OpenAlex.
- Functionalized zeolite regulates bone metabolic microenvironment.Materials today. Bio · 2025Review
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
5 authors at 3 institutions in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
The aim of this study was to evaluate the biocompatibility and osteogenic potential of a Zeolite Socony Mobil-5 (ZSM-5) coating on a Ti-24 Nb-4 Zr-7.9 Sn (Ti-2448) surface. ZSM-5-modified Ti-2448 (ZSM-5/Ti-2448) and Ti-2448 (control) groups were employed. The physical and chemical properties of the two types of samples were evaluated by scanning electron microscopy, Fourier-transform infrared spectroscopy, nitrogen adsorption/desorption, and contact angle methods. The surface of the ZSM-5/Ti-2448 was rougher than that of the original Ti-2448, while the contact angle of the ZSM-5/Ti-2448 was smaller than that of Ti-2448. In addition, the ZSM-5/Ti-2448 largely increased the specific surface area and introduced silanol groups. A bone-like apatite layer could be formed on the surface of ZSM-5/Ti-2448 after 14 days of incubation in a simulated body fluid. ZSM-5/Ti-2448 was not cytotoxic. The number and alkaline phosphatase (ALP) activity of osteoblasts on ZSM-5/Ti-2448 were significantly higher than those on Ti-2448 surfaces, obtained