ArticleACS biomaterials science & engineering2021
Characterization of Partially Covered Self-Expandable Metallic Stents for Esophageal Cancer Treatment:
Article in ACS biomaterials science & engineering, 2021. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
3 citing papers in PubMed, 10 citations in OpenAlex.
- The Impact of Internal Stress and Annealing on the Oxidation Stability of Polyurethane.Polymer science & technology (Washington, D.C.) · 2026Article
- Manufacturing, Processing, and Characterization of Self-Expanding Metallic Stents: A Comprehensive Review.Bioengineering (Basel, Switzerland) · 2024Review
- Advances in the development of biodegradable coronary stents: A translational perspective.Materials today. Bio · 2022Review
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
6 authors at 2 institutions in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
Partially covered self-expandable metallic esophageal stent (SEMS) placement is the most frequently applied palliative treatment in esophageal cancer. Structural characterization of explanted 16 nitinol-polyurethane SEMS (the group of 6 females, 10 males, age 40-80) was performed after their removal due to dysfunction. The adverse bulk changes in the polymer structure were identified using differential scanning calorimetry (DSC), differential mechanical thermal analysis (DMTA), and attenuated total reflectance infrared spectroscopy (ATR-IR) and discussed in terms of melting point shift (9 °C), glass-transition shift (4 °C), differences in viscoelastic behavior, and systematic decrease of peaks intensities corresponding to C-H, C═O, and C-N polyurethane structural bonds. The scanning electron and confocal microscopic observations revealed all major types of surface degradation, i.e., surface cracks, peeling off of the polymer material, and surface etching. The changes in the hydrophobic polyurethane surfaces were also revealed by a significant decrease in wettability (74°) and the corresponding increase of the surface free energy (31 mJ/m