Evidence map›Paper›PMID 33535590›Full record

ArticleMaterials (Basel, Switzerland)2021

Impact of Glass Composition on Hydrolytic Degradation of Polylactide/Bioactive Glass Composites.

Inari Lyyra, Katri Leino, Terttu Hukka, Markus Hannula, Minna Kellomäki, Jonathan Massera

Abstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2021. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 7 papers.

0numbers the graph read from it
0cells of the map it votes in
7citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

7 citing papers in PubMed.

  1. Review
  2. Review
  3. Article
  4. Article
  5. Article
  6. Bone Regeneration and Oxidative Stress: An Updated Overview.Antioxidants (Basel, Switzerland) · 2022
    Review
  7. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors.

Inari LyyraFaculty of Medicine and Health Technology, Tampere University, 33720 Tampere, Finland.
Katri LeinoFaculty of Medicine and Health Technology, Tampere University, 33720 Tampere, Finland.
Terttu HukkaFaculty of Engineering and Natural Sciences, Tampere University, 33720 Tampere, Finland.ORCID 0000-0001-6926-9743
Markus HannulaFaculty of Medicine and Health Technology, Tampere University, 33720 Tampere, Finland.
Minna KellomäkiFaculty of Medicine and Health Technology, Tampere University, 33720 Tampere, Finland.ORCID 0000-0003-4321-1820
Jonathan MasseraFaculty of Medicine and Health Technology, Tampere University, 33720 Tampere, Finland.

Funding

Academy of Finland 275427, 284492. and 312 409FINNISH FOUNDATION FOR TECHNOLOGY PROMOTION noneINDUSTRIAL RESEARCH FUND AT TAMPERE UNIVERSITY OF TECHNOLOGY NoneJane ja Aatos Erkon Säätiö AGATE
6 · The paper itself

Abstract

Understanding the degradation of a composite material is crucial for tailoring its properties based on the foreseen application. In this study, poly-L,DL-lactide 70/30 (PLA70) was compounded with silicate or phosphate bioactive glass (Si-BaG and P-BaG, respectively). The composite processing was carried out without excessive thermal degradation of the polymer and resulted in porous composites with lower mechanical properties than PLA70. The loss in mechanical properties was associated with glass content rather than the glass composition. The degradation of the composites was studied for 40 weeks in Tris buffer solution Adding Si-BaG to PLA70 accelerated the polymer degradation in vitro more than adding P-BaG, despite the higher reactivity of the P-BaG. All the composites exhibited a decrease in mechanical properties and increased hydrophilicity during hydrolysis compared to the PLA70. Both glasses dissolved through the polymer matrix with a linear, predictable release rate of ions. Most of the P-BaG had dissolved before 20 weeks in vitro, while there was still Si-BaG left after 40 weeks. This study introduces new polymer/bioactive glass composites with tailorable mechanical properties and ion release for bone regeneration and fixation applications.

Indexed as

bioactive glasscompositeshydrolytic degradationin vitroion releasemechanical propertiesmechanical strengthmolar masspolylactidethermal degradation

Identifiers

PMID33535590
PMCPMC7867177

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390