ArticleMaterials (Basel, Switzerland)2020

Surface Characterization and Conductivity of Two Types of Lithium-Based Glass Ceramics after Accelerating Ageing.

Marko Jakovac, Teodoro Klaser, Borna Radatović, Željko Skoko, Luka Pavić, Mark Žic

Open access · goldAbstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2020. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 10 papers.

0numbers the graph read from it
0cells of the map it votes in
10citing papers in PubMed
0.7field-weighted citation impact, top 41% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

10 citing papers in PubMed, 12 citations in OpenAlex.

  1. Article
  2. Article
  3. Article
  4. Article
  5. Article
  6. Article
  7. Article
  8. The Effect of YMaterials (Basel, Switzerland) · 2022
    Article
  9. Humidity Sensing Ceria Thin-Films.Nanomaterials (Basel, Switzerland) · 2022
    Article
  10. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors at 3 institutions in 1 country.

Marko JakovacDepartment of Prosthodontics, School of Dental Medicine, University Zagreb, 10000 Zagreb, Croatia.
Teodoro KlaserDepartment of Physics, Faculty of Science, University of Zagreb, 10000 Zagreb, Croatia.
Borna RadatovićCenter for Excellence for Advanced Materials and Sensing Devices, Institute of Physics, 10000 Zagreb, Croatia.
Željko SkokoDepartment of Physics, Faculty of Science, University of Zagreb, 10000 Zagreb, Croatia.ORCID 0000-0003-3000-7353
Luka PavićRuđer Bošković Institute, P.O. Box 180, 10000 Zagreb, Croatia.ORCID 0000-0003-2232-6602
Mark ŽicRuđer Bošković Institute, P.O. Box 180, 10000 Zagreb, Croatia.
University of Zagreb · HRRuđer Bošković Institute · HRInstitute of Physics · HR

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

In this study, two different dental ceramics, based on zirconia-reinforced lithium-silicate (LS1) glass-ceramics (Celtra Duo, Dentsply Sirona, Bensheim, Germany) and lithium disilicate (LS2) ceramics (IPS e.max CAD, Ivoclar, Vivadent, Schaan, Liechtenstein) were examined. They were tested prior to and after the crystallization by sintering in the dental furnace. Additionally, the impact of ageing on ceramic degradability was investigated by immersing it in 4% acetic acid at 80 °C for 16 h. The degradability of the materials was monitored by Impedance Spectroscopy (IS), X-Ray Powder Diffraction (XRPD), and Field Emission Scanning Electron Microscope (FE-SEM) techniques. It was detected that LS2 (vs. LS1) samples had a lower conductivity, which can be explained by reduced portions of structural defects. XRPD analyses also showed that the ageing increased the portion of defects in ceramics, which facilitated the ion diffusion and degradation of samples. To summarize, this study suggests that the non-destructive IS technique can be employed to probe the ageing properties of the investigated LS1 and LS2 ceramics materials.

Indexed as

acetic acidageingconductivitydegradationglass ceramicsimpedancelithium disilicateSEMXRPDzirconia-reinforced lithium silicate

Identifiers

PMID33321786
PMCPMC7763873
OpenAlexW3111441972

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.