Evidence map›Paper›PMID 32977513›Full record

ArticleMaterials (Basel, Switzerland)2020

Impact of Wound Closure on the Corrosion Rate of Biodegradable Mg-Ca-Zn Alloys in the Oral Environment.

Ali Modabber, Daniela Zander, Naemi Zumdick, Daniel Schick, Kristian Kniha, Stephan Christian Möhlhenrich, Frank Hölzle, Evgeny Goloborodko

Open access · goldAbstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2020. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.

0numbers the graph read from it
0cells of the map it votes in
3citing papers in PubMed
0.2field-weighted citation impact, top 49% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

3 citing papers in PubMed, 6 citations in OpenAlex.

  1. Review
  2. Bioactive materials · 2023
    Article
  3. Review
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

8 authors at 2 institutions in 1 country.

Ali ModabberDepartment of Oral, Maxillofacial and Facial Plastic Surgery, RWTH Aachen University Hospital, Pauwelsstr. 30, 52074 Aachen, Germany.ORCID 0000-0003-2160-4527
Daniela ZanderChair of Corrosion and Corrosion Protection, Foundry Institute Aachen, Division of Materials Science and Engineering, RWTH Aachen University, Intzestr. 5, 52072 Aachen, Germany.
Naemi ZumdickChair of Corrosion and Corrosion Protection, Foundry Institute Aachen, Division of Materials Science and Engineering, RWTH Aachen University, Intzestr. 5, 52072 Aachen, Germany.
Daniel SchickDepartment of Intensive Care Medicine, Medical Faculty, RWTH Aachen University, Pauwelsstr. 30, 52074 Aachen, Germany.
Kristian KnihaDepartment of Oral, Maxillofacial and Facial Plastic Surgery, RWTH Aachen University Hospital, Pauwelsstr. 30, 52074 Aachen, Germany.ORCID 0000-0001-8579-2622
Stephan Christian MöhlhenrichDepartment of Orthodontics, University of Witten/Herdecke, Alfred-Herrhausen Str. 50, 58448 Witten, Germany.ORCID 0000-0002-7023-991X
Frank HölzleDepartment of Oral, Maxillofacial and Facial Plastic Surgery, RWTH Aachen University Hospital, Pauwelsstr. 30, 52074 Aachen, Germany.
Evgeny GoloborodkoDepartment of Oral, Maxillofacial and Facial Plastic Surgery, RWTH Aachen University Hospital, Pauwelsstr. 30, 52074 Aachen, Germany.
RWTH Aachen University · DEWitten/Herdecke University · DE

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Magnesium alloys have exhibited a rapid rate of corrosion and thus early implant failure, so this study was designed to investigate the longer-term effects and in particular on wound closure. The aim of the study is to evaluate Mg-Ca-Zn Alloys as promising biodegradable implants in the field of maxillofacial surgery, which have so far never been evaluated for the changing conditions from a saliva to a serum-like environment after wound closure. Magnesium-0.6/calcium-0.8 wt.% zinc alloys were either immersed for 10 days in artificial saliva or 10 days in Hank's salt solution as control groups. The test group was transferred from artificial saliva to Hank's salt solution after 5 days in order to simulate wound closure. Corrosion rates were determined by immersion testing. Additional electron microscopy and energy dispersive X-ray spectroscopy (EDX) were performed. Prior artificial saliva exposure led to significantly decreased (

Indexed as

artificial salivabiodegradable implantscorrosionMg-Ca-Zn alloyswound closure

Identifiers

PMID32977513
PMCPMC7579560
OpenAlexW3089223792

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.