Evidence map›Paper›PMID 32917049›Full record

ArticleMaterials (Basel, Switzerland)2020

Gradient Microstructure Induced by Surface Mechanical Attrition Treatment (SMAT) in Magnesium Studied Using Positron Annihilation Spectroscopy and Complementary Methods.

Konrad Skowron, Ewa Dryzek, Mirosław Wróbel, Paweł Nowak, Marianna Marciszko-Wiąckowska, Léa Le Joncour, Manuel François, Benoit Panicaud, Andrzej Baczmański

Abstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2020. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 5 papers.

0numbers the graph read from it
0cells of the map it votes in
5citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

5 citing papers in PubMed.

  1. Review
  2. Review
  3. Article
  4. A review on magnesium alloys for biomedical applications.Frontiers in bioengineering and biotechnology · 2022
    Review
  5. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

9 authors.

Konrad SkowronInstitute of Nuclear Physics, Polish Academy of Sciences, PL-31342 Kraków, Poland.ORCID 0000-0003-1933-5452
Ewa DryzekInstitute of Nuclear Physics, Polish Academy of Sciences, PL-31342 Kraków, Poland.ORCID 0000-0002-2515-7843
Mirosław WróbelFaculty of Metals Engineering and Industrial Computer Science, AGH University of Science and Technology, al. A. Mickiewicza 30, 30-059 Kraków, Poland.
Paweł NowakJerzy Haber Institute of Catalysis and Surface Chemistry, Polish Academy of Sciences, Niezapominajek 8, PL-30239 Kraków, Poland.ORCID 0000-0003-2068-7068
Marianna Marciszko-WiąckowskaAcademic Centre for Materials and Nanotechnology, AGH University of Science and Technology, al. A. Mickiewicza 30, 30-059 Kraków, Poland.ORCID 0000-0003-3490-4422
Léa Le JoncourUniversité de Technologie de Troyes (UTT), LASMIS, 12 Rue Marie Curie, 10010 Troyes, France.
Manuel FrançoisUniversité de Technologie de Troyes (UTT), LASMIS, 12 Rue Marie Curie, 10010 Troyes, France.
Benoit PanicaudUniversité de Technologie de Troyes (UTT), LASMIS, 12 Rue Marie Curie, 10010 Troyes, France.
Andrzej BaczmańskiFaculty of Physics and Applied Computer Science, AGH University of Science and Technology, al. A. Mickiewicza 30, 30-059 Kraków, Poland.

Funding

EU POWR.03.02.00-00-I013/16
6 · The paper itself

Abstract

Surface mechanical attrition treatment (SMAT) was used to generate a gradient microstructure in commercial grade magnesium. Positron annihilation lifetime spectroscopy and variable energy positron beam measurements, as well as microhardness tests, electron backscatter diffraction, X-ray diffraction, and electrochemical corrosion tests, were used to investigate the created subsurface microstructure and its properties. It was found that SMAT causes an increase in dislocation density and grain refinement which results in increased hardness of the subsurface zone. The mean positron lifetime values indicate trapping of positrons in vacancies associated with dislocations and dislocation jogs. The increase of the SMAT duration and the vibration amplitude influences the depth profile of the mean positron lifetime, which reflects the defect concentration profile. Electrochemical measurements revealed that the structure induced by SMAT increases the susceptibility of magnesium to anodic oxidation, leading to the enhanced formation of hydroxide coverage at the surface and, as a consequence, to the decrease in corrosion current. No significant effect of the treatment on the residual stress was found.

Indexed as

corrosiongradient structured materialsmagnesiumpositron annihilation spectroscopySMATsurface mechanical attrition treatment

Identifiers

PMID32917049
PMCPMC7558138

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.