Biodegradation behavior of micro-arc oxidation coating on magnesium alloy-from a protein perspective.

Zhao-Qi Zhang, Li Wang, Mei-Qi Zeng, Rong-Chang Zeng, M Bobby Kannan, Cun-Guo Lin, Yu-Feng Zheng

Open access · goldAbstract read
In one paragraph

Article in Bioactive materials, 2020. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 20 papers.

0numbers the graph read from it
0cells of the map it votes in
20citing papers in PubMed
7.2field-weighted citation impact, top 2% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

20 citing papers in PubMed, 126 citations in OpenAlex.

  1. Article
  2. Review
  3. Review
  4. Article
  5. Article
  6. Review
  7. Review
  8. Review
  9. Article
  10. Review
  11. Review
  12. Article
  13. Review
  14. Review
  15. Review
  16. Article
  17. Article
  18. Article
  19. Microbial ingress andBioactive materials · 2020
    Article
  20. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

7 authors at 5 institutions in 2 countries.

Zhao-Qi ZhangCorrosion Laboratory for Light Metals, College of Material Science and Engineering, Shandong University of Science and Technology, Qingdao, 266590, China.
Li WangState Key Laboratory for Marine Corrosion and Protection, Luoyang Ship Material Research Institute, Qingdao, 266101, China.
Mei-Qi ZengCorrosion Laboratory for Light Metals, College of Material Science and Engineering, Shandong University of Science and Technology, Qingdao, 266590, China.
Rong-Chang ZengCorrosion Laboratory for Light Metals, College of Material Science and Engineering, Shandong University of Science and Technology, Qingdao, 266590, China.
M Bobby KannanBiomaterials and Engineering Materials (BEM) Laboratory, College of Science, Technology and Engineering, James Cook University, Townsville, 4811, Australia.
Cun-Guo LinState Key Laboratory for Marine Corrosion and Protection, Luoyang Ship Material Research Institute, Qingdao, 266101, China.
Yu-Feng ZhengState Key Laboratory for Turbulence and Complex Systems and Department of Materials Science and Engineering, College of Engineering, Peking University, Beijing, 100871, China.
China State Shipbuilding (China) · CNJames Cook University · AUPeking University · CNShandong University of Science and Technology · CNZhengzhou University · CN

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Protein exerts a critical influence on the degradation behavior of absorbable magnesium (Mg)-based implants. However, the interaction mechanism between protein and a micro-arc oxidation (MAO) coating on Mg alloys remains unclear. Hereby, a MAO coating was fabricated on AZ31 Mg alloy. And its degradation behavior in phosphate buffer saline (PBS) containing bovine serum albumin (BSA) was investigated and compared with that of the uncoated alloy. Surface morphologies and chemical compositions were studied using Field-emission scanning electron microscope (FE-SEM), Fourier transform infrared spectrophotometer (FT-IR) and X-ray diffraction (XRD). The degradation behavior of the bare Mg alloy and its MAO coating was studied through electrochemical and hydrogen evolution tests. Cytotoxicity assay was applied to evaluate the biocompatibility of Mg alloy substrate and MAO coating. Results indicated that the presence of BSA decreased the degradation rate of Mg alloy substrate because BSA (RCH(NH

Indexed as

BiocompatibilityDegradationMagnesium alloyMicro-arc oxidationProtein

Identifiers

PMID32258829
PMCPMC7113626
OpenAlexW3014557492

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC-ND
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.