Degradation properties of a biodegradable shape memory elastomer, poly(glycerol dodecanoate), for soft tissue repair.

Harsha Ramaraju, Loran D Solorio, Martin L Bocks, Scott J Hollister

Open access · goldAbstract read
In one paragraph

Article in PloS one, 2020. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 13 papers.

0numbers the graph read from it
0cells of the map it votes in
13citing papers in PubMed
1.9field-weighted citation impact, top 16% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

13 citing papers in PubMed, 28 citations in OpenAlex.

  1. Article
  2. Review
  3. Review
  4. Review
  5. Article
  6. Article
  7. Article
  8. Article
  9. Article
  10. Article
  11. Article
  12. Article
  13. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

4 authors at 3 institutions in 1 country.

Harsha RamarajuWallace H. Coulter Department of Biomedical Engineering, Georgia Institute of Technology, Atlanta, Georgia, United States of America.ORCID 0000-0001-9452-9228
Loran D SolorioDepartment of Biomedical Engineering, University of Michigan, Ann Arbor, Michigan, United States of America.
Martin L BocksUH Rainbow Babies & Children's Hospital, School of Medicine, Case Western Reserve University, Cleveland, Ohio, United States of America.ORCID 0000-0002-2778-5739
Scott J HollisterWallace H. Coulter Department of Biomedical Engineering, Georgia Institute of Technology, Atlanta, Georgia, United States of America.
Georgia Institute of Technology · USRainbow Babies & Children's Hospital · USUniversity of Michigan · US

Funding

PGD: A shape memory degradable polymer for transcatheter atrial septal defect closureR21HL126004 · NHLBI · UNIVERSITY OF MICHIGAN AT ANN ARBOR · PI HOLLISTER, SCOTT J · 2016 to 2017
$398k
NHLBI NIH HHS R21 HL126004
6 · The paper itself

Abstract

Development of biodegradable shape memory elastomers (SMEs) is driven by the growing need for materials to address soft tissue pathology using a minimally invasive surgical approach. Composition, chain length and crosslinking of biocompatible polymers like PCL and PLA have been investigated to control mechanical properties, shape recovery and degradation rates. Depending on the primary mechanism of degradation, many of these polymers become considerably stiffer or softer resulting in mechanical properties that are inappropriate to support the regeneration of surrounding soft tissues. Additionally, concerns regarding degradation byproducts or residual organic solvents during synthesis accelerated interest in development of materials from bioavailable monomers. We previously developed a biodegradable SME, poly(glycerol dodecanoate) (PGD), using biologically relevant metabolites and controlled synthesis conditions to tune mechanical properties for soft tissue repair. In this study, we investigate the influence of crosslinking density on the mechanical and thermal properties of PGD during in vitro and in vivo degradation. Results suggest polymer degradation in vivo is predominantly driven by surface erosion, with no significant effects of initial crosslinking density on degradation time under the conditions investigated. Importantly, mechanical integrity is maintained during degradation. Additionally, shifts in melt transitions on thermograms indicate a potential shift in shape memory transition temperatures as the polymers degrade. These findings support the use of PGD for soft tissue repair and warrant further investigation towards tuning the molecular and macromolecular properties of the polymer to tailor degradation rates for specific clinical applications.

Indexed as

Biocompatible MaterialsCalorimetryElastomersPolyestersPolymersTissue EngineeringTissue ScaffoldsBiocompatible MaterialsElastomersPolyesterspoly(glycerol-dodecanoate)Polymers

Identifiers

PMID32084184
PMCPMC7034845
OpenAlexW3007572672

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.