Evidence map›Paper›PMID 32051734›Full record

ArticleAmerican journal of translational research2020

Comparative assessment of the biocompatibility and degradation behavior of Zn-3Cu and JDBM alloys used for biliary surgery.

Sumin Chen, Lanting Yu, Qiuyan Zhao, Yingchun Ren, Lili Guo, Xiaoyuan Gong, Xinjian Wan, Guangyin Yuan, Baiwen Li

Open access · greenAbstract read
In one paragraph

Article in American journal of translational research, 2020. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.

0numbers the graph read from it
0cells of the map it votes in
3citing papers in PubMed
0.4field-weighted citation impact, top 45% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

3 citing papers in PubMed, 6 citations in OpenAlex.

  1. Review
  2. Article
  3. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

9 authors at 2 institutions in 1 country.

Sumin ChenDepartment of Gastroenterology, Tongren Hospital, Shanghai Jiao Tong University School of Medicine Shanghai, China.
Lanting YuDepartment of Gastroenterology, Shanghai General Hospital, Shanghai Jiao Tong University School of Medicine Shanghai 200233, China.
Qiuyan ZhaoDepartment of Gastroenterology, Shanghai General Hospital, Shanghai Jiao Tong University School of Medicine Shanghai 200233, China.
Yingchun RenDepartment of Gastroenterology, Shanghai General Hospital, Shanghai Jiao Tong University School of Medicine Shanghai 200233, China.
Lili GuoDepartment of Gastroenterology, Shanghai General Hospital, Shanghai Jiao Tong University School of Medicine Shanghai 200233, China.
Xiaoyuan GongDepartment of Gastroenterology, Shanghai General Hospital, Shanghai Jiao Tong University School of Medicine Shanghai 200233, China.
Xinjian WanShanghai Sixth People's Hospital, Shanghai Jiaotong University Shanghai 200233, China.
Guangyin YuanNational Engineering Research Center of Light Alloy Net Forming and State Key Laboratory of Metal Matrix Composite, Shanghai Jiao Tong University Shanghai 200240, China.
Baiwen LiDepartment of Gastroenterology, Shanghai General Hospital, Shanghai Jiao Tong University School of Medicine Shanghai 200233, China.
Shanghai Jiao Tong University · CNShanghai Sixth People's Hospital · CN

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

This study was designed to investigate the biocompatibility and the degradation behavior of a Zn-3Cu alloy, a Zn-3Cu coating alloy, a Mg-Nd-Zn-Zr (denoted as JDBM) alloy and a JDBM coating alloy to choose the optimal alloy for common bile duct (CBD) surgery. In the in vitro degradation experiments, we observed the surface morphology of the samples and determined the elements of the corrosion products. In the in vitro cytotoxicity experiments, the cell morphology and cytotoxicity were observed and tested. In the in vivo experiments, in addition to analyzing the samples, we also analyzed the variations in serum magnesium, serum creatinine (CREA), blood urea nitrogen (BUN), total bilirubin (TB) and glutamic pyruvic transaminase (GPT). Moreover, important tissue samples from the CBD, liver, kidney and spleen were taken for histological evaluation. The in vitro degradation experiments revealed that the surface corrosion of the JDBM and JDBM coating alloys were more obvious than that of Zn-3Cu and Zn-3Cu coating alloys, and the degradation rate of the JDBM coating alloy was the slowest. The in vitro cytotoxicity assessment showed that the JDBM alloy and JDBM coating alloy extracts were biologically safe for L-929 cells, while the Zn-3Cu alloy and Zn-3Cu coating alloy extracts were harmful to L-929 cells. In the in vivo experiments, neither the JDBM alloy nor the JDBM coating alloy affected the function or morphology of the bile duct, liver, kidney or spleen. Similar to the in vitro degradation behavior, the surface corrosion of the JDBM alloy was more significant than that of the JDBM coating alloy. Our data suggested that the JDBM coating alloy is a safe, biodegradable material for CBD surgery.

Indexed as

biocompatibilitycommon bile duct surgerydegradation behaviorMagnesium alloys

Identifiers

PMID32051734
PMCPMC7013214
OpenAlexW3008047606

What OpenQuestion holds

Textmetadata
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.