Evidence map›Paper›PMID 31181799›Full record

ArticlePolymers2019

Degradation Behavior In Vitro of Carbon Nanotubes (CNTs)/Poly(lactic acid) (PLA) Composite Suture.

Shuqiang Liu, Gaihong Wu, Xiaogang Chen, Xiaofang Zhang, Juanjuan Yu, Mingfang Liu, Yao Zhang, Peng Wang

Abstract read
In one paragraph

Article in Polymers, 2019. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 26 papers.

0numbers the graph read from it
0cells of the map it votes in
26citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

26 citing papers in PubMed.

  1. Article
  2. Article
  3. Review
  4. Article
  5. Article
  6. Review
  7. Article
  8. Article
  9. Review
  10. Review
  11. Review
  12. Article
  13. Article
  14. Comparison of the Dielectric Properties of EcoflexMaterials (Basel, Switzerland) · 2021
    Article
  15. Article
  16. Article
  17. Article
  18. Article
  19. Article
  20. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

8 authors.

Shuqiang LiuCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. liushuqiang8866@126.com.
Gaihong WuCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. gaigai2003@126.com.
Xiaogang ChenSchool of Materials, The University of Manchester, Manchester M13 9PL, UK. xiaogang.chen@manchester.ac.uk.ORCID 0000-0001-5223-2397
Xiaofang ZhangCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. xiaofangfang521a@163.com.
Juanjuan YuCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. yuxiaoyuy@126.com.
Mingfang LiuCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. lmf118119@163.com.
Yao ZhangCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. zy32164872@126.com.
Peng WangCollege of Textile Engineering, Taiyuan University of Technology, Taiyuan 030024, China. tyut19834520797@163.com.

Funding

2017 Shanxi Philosophy and Social Science Project 201702MOE (Ministry of Education in China) Project of Humanities and Social Sciences 18YJC760051Program for the Philosophy and Social Sciences Research of Higher Learning Institutions of Shanxi (PSSR) 201803060Scientific and Technological Innovation Programs of Higher Education Institutions in Shanxi 2015125Shanxi University Students Innovation and Entrepreneurship Training Program Project 2018099Students Innovation and Entrepreneurship Training Program Project of Taiyuan University of Technology 18049Youth Foundation of Taiyuan University of Technology 2015QN042
6 · The paper itself

Abstract

Poly(lactic acid) (PLA) suture can be absorbed by the human body, and so have wide applications in modern surgery operations. The degradation period of PLA suture is expected to meet with the healing time of different types of wounds. In order to control the degradation period of the PLA suture, the carbon nanotubes (CNTs) were composited with PLA suture, and the degradation experiment in vitro was performed on sutures. The structure and properties of sutures during degradation, such as surface morphology, breaking strength, elongation, mass and chemical structure, were tracked and analyzed. The results indicated that the degradation brought about surface defects and resulted in 13.5 weeks for the strength valid time of the original PLA suture. By contrast, the strength valid time of the CNTs/PLA suture was increased to 26.6 weeks. Whilst the toughness of both the pure PLA and CNTs/PLA sutures decreased rapidly and almost disappeared after 3 to 4 weeks of degradation. The mass loss demonstrated that the time required for complete degradation of the two sutures was obviously different, the pure PLA suture 49 weeks, while CNTs/PLA sutures 63 to 73 weeks. The research proved that CNTs delayed PLA degradation and prolonged its strength valid time in degradation.

Indexed as

carbon nanotubescomposite suturedegradation behaviorpoly(lactic acid)

Identifiers

PMID31181799
PMCPMC6630379

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.