Evidence map›Paper›PMID 28746397›Full record

ArticlePloS one2017

Biocide-mediated corrosion of coiled tubing.

Mohita Sharma, Dongshan An, Tao Liu, Tijan Pinnock, Frank Cheng, Gerrit Voordouw

Open access · goldAbstract read
In one paragraph

Article in PloS one, 2017. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 4 papers.

0numbers the graph read from it
0cells of the map it votes in
4citing papers in PubMed
1.5field-weighted citation impact, top 19% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

4 citing papers in PubMed, 19 citations in OpenAlex.

  1. Article
  2. Article
  3. Article
  4. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors at 1 institution in 1 country.

Mohita SharmaPetroleum Microbiology Research Group, Department of Biological Sciences, University of Calgary, Alberta, Canada.ORCID http://orcid.org/0000-0003-2584-3074
Dongshan AnPetroleum Microbiology Research Group, Department of Biological Sciences, University of Calgary, Alberta, Canada.
Tao LiuDepartment of Mechanical and Manufacturing Engineering, University of Calgary, Calgary, Alberta, Canada.
Tijan PinnockPetroleum Microbiology Research Group, Department of Biological Sciences, University of Calgary, Alberta, Canada.
Frank ChengDepartment of Mechanical and Manufacturing Engineering, University of Calgary, Calgary, Alberta, Canada.
Gerrit VoordouwPetroleum Microbiology Research Group, Department of Biological Sciences, University of Calgary, Alberta, Canada.
University of Calgary · CA

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Coiled tubing corrosion was investigated for 16 field water samples (S5 to S20) from a Canadian shale gas field. Weight loss corrosion rates of carbon steel beads incubated with these field water samples averaged 0.2 mm/yr, but injection water sample S19 had 1.25±0.07 mm/yr. S19 had a most probable number of zero acid-producing bacteria and incubation of S19 with carbon steel beads or coupons did not lead to big changes in microbial community composition. In contrast other field water samples had most probable numbers of APB of 102/mL to 107/mL and incubation of these field water samples with carbon steel beads or coupons often gave large changes in microbial community composition. HPLC analysis indicated that all field water samples had elevated concentrations of bromide (average 1.6 mM), which may be derived from bronopol, which was used as a biocide. S19 had the highest bromide concentration (4.2 mM) and was the only water sample with a high concentration of active bronopol (13.8 mM, 2760 ppm). Corrosion rates increased linearly with bronopol concentration, as determined by weight loss of carbon steel beads, for experiments with S19, with filtered S19 and with bronopol dissolved in defined medium. This indicated that the high corrosion rate found for S19 was due to its high bronopol concentration. The corrosion rate of coiled tubing coupons also increased linearly with bronopol concentration as determined by electrochemical methods. Profilometry measurements also showed formation of multiple pits on the surface of coiled tubing coupon with an average pit depth of 60 μm after 1 week of incubation with 1 mM bronopol. At the recommended dosage of 100 ppm the corrosiveness of bronopol towards carbon steel beads was modest (0.011 mm/yr). Higher concentrations, resulting if biocide is added repeatedly as commonly done in shale gas operations, are more corrosive and should be avoided. Overdosing may be avoided by assaying the presence of residual biocide by HPLC, rather than by assaying the presence of residual surviving bacteria.

Indexed as

CorrosionSteelWater MicrobiologyBacteriaBromidesCanadaCarbonChromatography, High Pressure LiquidDisinfectantsDNA Barcoding, TaxonomicOil and Gas FieldsPopulation DensityPopulation DynamicsPropylene GlycolsRNA, Ribosomal, 16SWaterBromidesbronopolCarbonDisinfectantsPropylene GlycolsRNA, Ribosomal, 16SSteelWater

Identifiers

PMID28746397
PMCPMC5528904
OpenAlexW2736997003

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.