Evidence map›Paper›PMID 26816655›Full record

ArticleRegenerative biomaterials2016

In vitro corrosion of pure magnesium and AZ91 alloy-the influence of thin electrolyte layer thickness.

Rong-Chang Zeng, Wei-Chen Qi, Fen Zhang, Shuo-Qi Li

Open access · goldAbstract read
In one paragraph

Article in Regenerative biomaterials, 2016. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 4 papers.

0numbers the graph read from it
0cells of the map it votes in
4citing papers in PubMed
1.2field-weighted citation impact, top 22% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

4 citing papers in PubMed, 14 citations in OpenAlex.

  1. Review
  2. Article
  3. Review
  4. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

4 authors at 1 institution in 1 country.

Rong-Chang ZengCollege of Materials Science and Engineering, Shandong University of Science and Technology, Qingdao 266590, China; State Key Laboratory of Mining Disaster Prevention and Control Co-Founded by Shandong Province and the Ministry of Science and Technology, Shandong University of Science and Technology, Qingdao 266590, China.
Wei-Chen QiCollege of Materials Science and Engineering, Shandong University of Science and Technology, Qingdao 266590, China; State Key Laboratory of Mining Disaster Prevention and Control Co-Founded by Shandong Province and the Ministry of Science and Technology, Shandong University of Science and Technology, Qingdao 266590, China.
Fen ZhangCollege of Materials Science and Engineering, Shandong University of Science and Technology, Qingdao 266590, China; State Key Laboratory of Mining Disaster Prevention and Control Co-Founded by Shandong Province and the Ministry of Science and Technology, Shandong University of Science and Technology, Qingdao 266590, China.
Shuo-Qi LiCollege of Materials Science and Engineering, Shandong University of Science and Technology, Qingdao 266590, China; State Key Laboratory of Mining Disaster Prevention and Control Co-Founded by Shandong Province and the Ministry of Science and Technology, Shandong University of Science and Technology, Qingdao 266590, China.
Shandong University of Science and Technology · CN

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

In vivo degradation predication faces a huge challenge via in vitro corrosion test due to the difficulty for mimicking the complicated microenvironment with various influencing factors. A thin electrolyte layer (TEL) cell for in vitro corrosion of pure magnesium and AZ91 alloy was presented to stimulate the in vivo corrosion in the micro-environment built by the interface of the implant and its neighboring tissue. The results demonstrated that the in vivo corrosion of pure Mg and the AZ91 alloy was suppressed under TEL condition. The AZ91 alloy was more sensitive than pure Mg to the inhibition of corrosion under a TEL thickness of less than 200 µm. The TEL thickness limited the distribution of current, and thus localized corrosion was more preferred to occur under TEL condition than in bulk solution. The TEL cell might be an appropriate approach to simulating the in vivo degradation of magnesium and its alloys.

Indexed as

biomaterialscorrosionmagnesiumthin electrolyte layer

Identifiers

PMID26816655
PMCPMC4723276
OpenAlexW2292936755

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.