ArticleJournal of biomedical materials research. Part B, Applied biomaterials2016

Degradation in the fatigue strength of dentin by diamond bur preparations: Importance of cutting direction.

B Majd, H Majd, J A Porter, E Romberg, D Arola

Abstract read
In one paragraph

Article in Journal of biomedical materials research. Part B, Applied biomaterials, 2016. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.

0numbers the graph read from it
0cells of the map it votes in
3citing papers in PubMed
1.1field-weighted citation impact, top 26% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

3 citing papers in PubMed, 9 citations in OpenAlex.

  1. Article
  2. The Tooth: Its Structure and Properties.Dental clinics of North America · 2017
    Review
  3. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

5 authors at 3 institutions in 1 country.

B MajdDepartment of Mechanical Engineering, University of Maryland Baltimore County, Baltimore, Maryland.
H MajdDepartment of Mechanical Engineering, University of Maryland Baltimore County, Baltimore, Maryland.
J A PorterDepartment of Endodontics, Prosthodontics and Operative Dentistry, Dental School, University of Maryland, Baltimore, Maryland.
E RombergDepartment of Endodontics, Prosthodontics and Operative Dentistry, Dental School, University of Maryland, Baltimore, Maryland.
D ArolaDepartment of Materials Science and Engineering, University of Washington, Seattle, Washington.
University of Maryland, Baltimore · USUniversity of Maryland, Baltimore County · USUniversity of Washington · US

Funding

Aging and Fatigue Crack Growth in DentinR01DE016904 · NIDCR · UNIVERSITY OF MARYLAND BALTIMORE COUNTY · PI AROLA, DWAYNE DALE · 2007 to 2010
$1.0M
NIDCR NIH HHS DE16904NIDCR NIH HHS R01 DE016904
6 · The paper itself

Abstract

The objectives of this investigation were to evaluate the degradation in fatigue strength of dentin by diamond bur preparations and to identify the importance of cutting direction. Three groups of coronal dentin specimens were prepared from unrestored third molars, including a flaw free "control," and two groups that received a diamond bur cutting treatment performed parallel or perpendicular to the specimen length. The specimens were subjected to static or cyclic flexural loading to failure and the results were compared with data for carbide bur cutting. Under static loading diamond bur cutting resulted in significantly lower flexure strength (p ≤ 0.05) than the control for both cutting directions (from 154 to ∼124 MPa). However, there was no significant difference in the strength between the control and carbide bur treated specimens. Similarly, the fatigue strength of the diamond bur treated specimens was significantly lower (p ≤ 0.0001) than that of the control for both cutting directions. Cutting in the perpendicular direction resulted in nearly 60% reduction to the endurance limit (from 44 to 19 MPa). Based on the results, diamond bur cutting of cavity preparations causes a reduction in the fatigue strength of dentin, regardless of the cutting direction. To maintain the durability of dentin, cavity preparations introduced using diamond burs must be performed with appropriate cutting direction and followed by a finishing pass.

Indexed as

Stress, MechanicalAdolescentAdultDentinDiamondFemaleHumansMaleMolarDiamondcuttingdentindiamond burfatiguetooth fracture

Identifiers

PMID25611951
PMCPMC4510045
OpenAlexW1549951247

What OpenQuestion holds

Textmetadata
LicenceTDM
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.