ArticleJournal of materials science. Materials in medicine2009
Preparation and characterization of biodegradable poly(D,L-lactide) and surface-modified bioactive glass composites as bone repair materials.
Article in Journal of materials science. Materials in medicine, 2009. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
5 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
In order to improve filler dispersion and phase compatibility between poly(D,L-lactide) (PDLLA) and inorganic bioactive glass (BG) particles, and to enhance the mechanical properties of PDLLA/BG composites, the silane coupling agent 3-glycidoxypropyltrimethoxysilane (KH570) was used to modify the surface of BG particles (represented by KBG). The structure and properties of PDLLA/BG and PDLLA/KBG composites were investigated by mechanical property testing and scanning electron microscopy (SEM). This study demonstrated that the Guth and Gold models can be combined to predict the Young's modulus of the composites. The Pukanszky modulus showed that the interaction parameter B of PDLLA/KBG composites was higher than that of the PDLLA/BG, which indicates that there is a higher interfacial interaction between the PDLLA and KBG. The composites were incubated in simulated body fluid (SBF) at 37 degrees C to study the in vitro degradation and bioactivity of the composites and to detect bone-like apatite formation on their surfaces.
Indexed as
Identifiers
19449200What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.