ArticleEnvironmental science and pollution research international2009
Weathering patinas on the medieval (S. XIV) stained glass windows of the Pedralbes Monastery (Barcelona, Spain).
Article in Environmental science and pollution research international, 2009. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 7 papers.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
7 citing papers in PubMed, 28 citations in OpenAlex.
- A Novel Approach to Carbonate Stone Conservation: Induced Calcium Oxalate Formation Through the Application of AmmoniumMolecules (Basel, Switzerland) · 2026Article
- AmmoniumMolecules (Basel, Switzerland) · 2023Article
- The Degradation of Daguerreotypes and the Relationship with Their Multi-Material Structure: A Multimodal Investigation.Sensors (Basel, Switzerland) · 2023Article
- Cultural heritage and its environment: an issue of interest for Environmental Science and Pollution Research.Environmental science and pollution research international · 2014Article
- Microscopic, chemical, and molecular-biological investigation of the decayed medieval stained window glasses of two Catalonian churches.International biodeterioration & biodegradation · 2013Article
- Patinas developed in environmental burial conditions: the Neolithic steles of Reguers de Seró (Lleida, Spain).Environmental science and pollution research international · 2010Article
- The enhanced deterioration of the cultural heritage monuments due to air pollution.Environmental science and pollution research international · 2009Article
Corrections and comments
- Commented on by
Authors and funding
6 authors at 3 institutions in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
BACKGROUND, AIM, AND SCOPE: The first step in the restoration of a medieval stained glass window is the evaluation of its degree of degradation. This implies the study of the chemical composition of the stained glass as well as the new mineral phases developed on its surface (patinas). Patinas are clearly related to glass composition, time, environmental conditions, microenvironments developed in local zones, bioactivity, physical and chemical factors, etc. This study was carried out on patinas developed in selected Na-rich stained glass of the Santa Maria de Pedralbes Monastery (Barcelona, Spain). The location of this monument in the city (about 5 km from the shoreline and close to the Collserola hill flank) helped to determine the environmental conditions in which patinas developed. The aim of our study was to characterize the patinas formed on the surface of the selected glass of this monastery in order to understand the role of the chemical composition of the original glass (Na-rich) as well as the environmental conditions in which they developed. MATERIALS AND
methodsPowdered samples of two different color-type patinas (ochre-orange and brownish) were collected in the external and internal parts of the stained glass windows of the Prebystery and Chapter House of the Pedralbes Monastery by using a precision (odontological) drill. These patinas were subsequently analyzed by X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR).
resultsXRD analyses evidenced the presence of sulfates (gypsum and thenardite), calcite, Ca-oxalates (whewellite and weddellite), and quartz forming part of the patinas. Although these mineral phases can be found in both color-type patinas, whewellite and thenardite are more common in the ochre-orange patinas. The results obtained were validated by the FTIR measurements. It has been observed, when thenardite is present, that gypsum occurs as traces. Thenardite is in most of the cases associated with whewellite and mainly occurs in the internal parts of the glass. In contrast, weddellite is limited to the absence of thenardite and whewellite and to the external parts of the stained glass. Quartz is present in all the patinas independent of their location and color. Calcite also occurs in many samples. It appears in both color-type patinas and, in some cases, is associated to the presence of weddellite but not to whewellite and/or thenardite. DISCUSSION: Glass composition together with environmental conditions and location of the patinas (internal or external parts of the stained glass window), as well as the provenance of the glass within the monastery, are the main factors that define the development of the new mineral phases. Moreover, the action of microorganisms, when present, can also strongly influence the development of some mineral phases. For example, the formation of calcite in the external parts of the stained glass (associated with the presence of oxalates) is related to the action of microorganisms. When calcite is formed in the internal parts of the glass and it is not associated with the presence of Ca-oxalates, an inorganic origin can be invoked. The presence of weddellite requires a very humid microenvironment with very little exposure to sunlight. In fact, this mineral phase has only been observed in the external parts of some glass located in the humid and shady side of the monastery. Whewellite (which only appears in the internal parts) needs a low degree of relative humidity. It has been observed that sulfur precipitating in basically one mineral phase (thenardite or gypsum) depends on the microenvironmental conditions of the moment and the glass composition. When thenardite occurs, it can be maintained that the original glass is of Na composition. The occurrence of quartz in all samples is interpreted as being due to the deposition of atmospheric particulate matter. The color of the patinas can be originated by different processes (presence of carotenes, organic pigmentation, atmospheric contamination, etc.).
conclusionsIn the case of moderately weathered stained glass windows, the combination of XRD and FTIR techniques is very useful to obtain a fast preliminary evaluation of the degree of weathering of a stained glass window. The presence of specific mineral phases in the patina (e.g., thenardite) confirms the Na composition of the original stained glass. This is important since Na-rich glass underwent a lesser degree of weathering than K- or K-Ca-rich glass. However, their absence cannot preclude other possibilities. It has been extensively evidenced through time that environmental conditions play an important role on the formation of the different mineral phases which form part of the patinas. RECOMMENDATIONS AND PERSPECTIVES: The first step in the restoration of a stained glass window is the evaluation of the degree of deterioration of the glass. This evaluation includes a chemical analysis of the glass as well as a characterization of the patinas developed on their surfaces. The obtained results will be essential in order to define the best restoration practices to be followed.